AerMet alloy is an ultra-high strength type of martensitic alloy steel. The main alloying elements are cobalt and nickel, but chromium, molybdenum and carbon are also added. Its exceptional properties are hardness, tensile strength, fracture toughness and ductility. Aermet is weldable with no preheating needed. AerMet alloy is not corrosion resistant, so it must be sealed if used in a moist environment. AerMet is a registered trademark of Carpenter Technology Corporation. Three types of AerMet alloys are currently available: AerMet 100 (also known as AerMet-for-Tooling), AerMet 310 and AerMet 340 alloy. Examples of applications include armor, fasteners, airplane landing gear, ordnance, jet engine shafts, structural members and drive shafts.
AerMet alloy is an ultra-high strength type of martensitic alloy steel. The main alloying elements are cobalt and nickel, but chromium, molybdenum and carbon are also added. Its exceptional properties are hardness, tensile strength, fracture toughness and ductility. Aermet is weldable with no preheating needed. AerMet alloy is not corrosion resistant, so it must be sealed if used in a moist environment. AerMet is a registered trademark of Carpenter Technology Corporation. Three types of AerMet alloys are currently available: AerMet 100 (also known as AerMet-for-Tooling), AerMet 310 and AerMet 340 alloy. Examples of applications include armor, fasteners, airplane landing gear, ordnance, jet engine shafts, structural members and drive shafts.
Properties
AerMet 310 Alloy
AerMet 310 is harder and stronger than AerMet 100 alloy while maintaining ductility and toughness. Standard shapes include round bar, wire, billet, plate, and strip. AerMet 310 is hardened with the same procedure as AerMet 100.
AerMet 340 Alloy
AerMet 340 alloy has a higher strength than AerMet 310. AerMet 340 is hardened differently from the other two varieties. The first hardening application is a solution treatment at for 1 hour. It is then quenched to a temperature of over 1 to 2 hours. The material may then be cold treated, where the material is cooled to for 1 hour. The second hardening process is aging, where the material is heated to for 3 to 8 hours. If the cold treatment is skipped, the part can be aged twice to get the same results.
See also
Maraging steel (Precipitation-hardened steels with similar strength.) USAF-96 and Eglin steel (Inexpensive precipitation-hardened steels with high strength and lower nickel content. USAF-96 also needs no tungsten.)