Bismanol is a magnetic alloy of bismuth and manganese (manganese bismuthide) developed by the US Naval Ordnance Laboratory.

Bismanol is a magnetic alloy of bismuth and manganese (manganese bismuthide) developed by the US Naval Ordnance Laboratory.

History

Bismanol, a permanent magnet made from powder metallurgy of manganese bismuthide, was developed by the US Naval Ordnance Laboratory in the early 1950s – at the time of invention it was one of the highest coercive force permanent magnets available, at 3000 oersteds. Coercive force reached 3650 oersteds and magnetic flux density 4800 by the mid 1950s. The material was generally strong, and stable to shock and vibration, but had a tendency to chip.

Slow corrosion of the material occurred under normal conditions. The material was used to make permanent magnets for use in small electric motors. Bismanol magnets have been replaced by neodymium magnets which are both cheaper and superior in other ways, by samarium-cobalt magnets in more critical applications, and by alnico magnets.

Text derived from https://en.wikipedia.org/w/index.php?oldid=1299208413 under CC BY-SA 4.0; modifications have been made.

Sources cited in this revision

1 named source(s) extracted from the cited revision. A source with no author is shown by its publication; nothing is invented.