Energetically modified cement

Uses your system voice; voice and rate in settings.

Snapshot

≈ 18 min read

Names in other languages

No names in other languages are held for this entry yet.

Article bodies are English and are not machine-translated. A name in another language is not a translation of the article.

, Sweden, 2020) Energetically modified cements (EMCs) are a class of cements made from pozzolans (e.g. fly ash, volcanic ash, pozzolana), silica sand, blast furnace slag, or Portland cement (or blends of these ingredients). The term "energetically modified" arises by virtue of the mechanochemistry process applied to the raw material, more accurately classified as "high energy ball milling" (HEBM).

At its simplest this means a milling method that invokes high kinetics by subjecting "powders to the repeated action of hitting balls" as compared to (say) the low kinetics of rotating ball mills. This causes, amongst others, a thermodynamic transformation in the material to increase its chemical reactivity. For EMCs, the HEBM process used is a unique form of specialised vibratory milling discovered in Sweden and applied only to cementitious materials, here called "EMC Activation".

By improving the reactivity of pozzolans, their strength-development rate is increased. This allows for compliance with modern product-performance requirements ("technical standards") for concretes and mortars. In turn, this allows for the replacement of Portland cement in the concrete and mortar mixes. This has a number of benefits to their long-term qualities. Energetically modified cements have a wide range of uses.…

, Sweden, 2020) Energetically modified cements (EMCs) are a class of cements made from pozzolans (e.g. fly ash, volcanic ash, pozzolana), silica sand, blast furnace slag, or Portland cement (or blends of these ingredients). The term "energetically modified" arises by virtue of the mechanochemistry process applied to the raw material, more accurately classified as "high energy ball milling" (HEBM).

At its simplest this means a milling method that invokes high kinetics by subjecting "powders to the repeated action of hitting balls" as compared to (say) the low kinetics of rotating ball mills. This causes, amongst others, a thermodynamic transformation in the material to increase its chemical reactivity. For EMCs, the HEBM process used is a unique form of specialised vibratory milling discovered in Sweden and applied only to cementitious materials, here called "EMC Activation".

By improving the reactivity of pozzolans, their strength-development rate is increased. This allows for compliance with modern product-performance requirements ("technical standards") for concretes and mortars. In turn, this allows for the replacement of Portland cement in the concrete and mortar mixes. This has a number of benefits to their long-term qualities. Energetically modified cements have a wide range of uses. For example, EMCs have been used in concretes for large infrastructure projects in the United States, meeting U.S. concrete standards.

Justification

(LTU) campus in Luleå, Sweden The term "energetically modified cement" incorporates a simple thermodynamic descriptor to refer to a class of cements produced using a specialised highly intensive milling process first discovered in 1992 at Luleå University of Technology (LTU) in Sweden. The transformatory process is initiated entirely mechanically as opposed to heating the materials directly. The mechanisms of mechanochemical transformations are often complex and different from "traditional" thermal or photochemical mechanisms.

HEBM can transform both the physical and thermodynamic properties that for example, "can lead to glass formation from elemental powder mixtures as well as by amorphization of intermetallic compound powders". The effects of HEBM-transformation cause a thermodynamic change that resides ultimately in a modified Gibbs Energy. The process increases the binding capacity and chemical reactivity rates of the materials transformed. Continuing academic work and research regarding "self-healing" properties of energetically modified cements is ongoing at LTU.

For example, EMCs has received awards from the Elsa ō Sven Thysells stiftelse för konstruktionsteknisk forskning (Elsa & Sven Thysell Foundation for Construction Engineering Research) of Sweden. The contribution of EMCs to the domain of mechanochemistry itself has also been recognised.

Etymology

The term "energetically modified cement" was first used in 1992 by Vladimir Ronin, introduced in a paper by Ronin et al. dated 1993 and presented at a formal meeting of the academic Nordic Concrete Research group. The process was refined by Ronin and others, including Lennart Elfgren (now Professor Emeritus of LTU, Department of Civil, Environmental and Natural Resources Engineering).

In 2023, LTU awarded Elfgren the "Vice-Chancellor's Medal for Merit for outstanding and meritorious work" by virtue of his work "...for the spread of new knowledge and understanding of, in particular, the concrete construction field". At the 45th World Exhibition of Invention, Research and Innovation, held in 1996 in Brussels, Belgium, EMC Activation was awarded a gold medal with mention by EUREKA, the European inter-governmental (research and development) organisation, for "modification énergique de ciments".

The term "energetically modified" has been used elsewhere—for example as recently as 2017—although such usage does not denote the method used was EMC Activation as defined here.

Overview

The claims made include: An EMC is a fine powder (typical of all cements) whose colour depends on the material processed. EMCs are produced using only a "fraction" of the energy used in Portland cement production (claimed ~100 KWh/tonne, C95). This comprised a "total cementitious content" of 335 kg/m^3 (564 lbs/CY) concrete mix.

Properties of concretes and mortars made from EMCs

Custom design for end-usage

The performance of mortars and concretes made from EMCs can be custom-designed. For example, EMC concretes can range from general application (for strength and durability) through to the production of rapid and ultra-rapid hardening high-strength concretes (for example, over 70 MPa / 10,150 psi in 24 hours and over 200 MPa / 29,000 psi in 28 days). This allows energetically modified cements to yield High Performance Concretes.

EMCs using California pozzolans

Concretes made by replacing at least 50% of the Portland cement with EMCs have yielded consistent field results in high-volume applications. This is also the case for EMC made from natural pozzolans (e.g., volcanic ash). Volcanic ash deposits from Southern California were independently tested; at 50% Portland cement replacement, the resulting concretes exceeded the requirements of the relevant US standard. At 28 days, the compressive strength was 4,180 psi / 28.8 MPa (N/mm²). The 56-day strength exceeded the requirements for 4,500 psi (31.1 MPa) concrete, even taking into account the safety margin as recommended by the American Concrete Institute. The concrete made in this way was workable and sufficiently strong, exceeding the 75% standard of pozzolanic activity at both 7 days and 28 days. The surface smoothness of pozzolans in the concrete was also increased.

Effect on pozzolanic reactions

, USA. EMC Activation is a process that increases a pozzolan's chemical affinity for pozzolanic reactions. This leads to faster and greater strength development of the resulting concrete, at higher replacement ratios, than untreated pozzolans. These transformed (now highly reactive pozzolans) demonstrate further benefits using known pozzolanic reaction-pathways that typically see as their end-goal a range of hydrated products.

An NMR study on EMCs concluded that EMC Activation caused "the formation of thin SiO 2 layers around C3S crystals", which in turn, "accelerates the pozzolanic reaction and promotes growing of more extensive nets of the hydrated products". In simple terms, by using pozzolans in concrete, porous (reactive) Portlandite can be transformed into hard and impermeable (relatively non-reactive) compounds, rather than the porous and soft relatively reactive calcium carbonate produced using ordinary cement.

Many of the end products of pozzolanic chemistry exhibit a hardness greater than 7.0 on the Mohs scale."Self healing" capabilities may also contribute to enhanced field-application durabilities where mechanical stresses may be present. In greater detail, the benefits of pozzolanic concrete, starts with an understanding that in concrete (including concretes with EMCs), Portland cement combines with water to produce a stone-like material through a complex series of chemical reactions, whose mechanisms are still not fully understood.

That chemical process, called mineral hydration, forms two cementing compounds in the concrete: calcium silicate hydrate (C-S-H) and calcium hydroxide (Ca(OH) 2 ).

This reaction can be noted in three ways, as follows: Standard notation:   Ca3SiO5 + H2O -> (CaO) * (SiO2) * (H2O) + Ca(OH)2 Balanced:   2Ca3SiO5 + 7H2O -> 3CaO * 2SiO2 * 4H2O + 3Ca(OH)2 Cement chemist notation (the hyphenation denotes the variable stoichiometry):  C 3 S  +  H   →   C-S-H  +  CH The underlying hydration reaction forms two products: Calcium silicate hydrate (C-S-H), which gives concrete its strength and dimensional stability.

The crystal structure of C-S-H in cement paste has not been fully resolved yet and there is still ongoing debate over its nanostructure. Calcium hydroxide (Ca(OH) 2 ), which in concrete chemistry is known also as Portlandite. In comparison to calcium silicate hydrate, Portlandite is relatively porous, permeable and soft (2 to 3, on Mohs scale). It is also sectile, with flexible cleavage flakes. Portlandite is soluble in water, to yield an alkaline solution which can compromise a concrete's resistance to acidic attack.

Portlandite makes up about 25% of concrete made with Portland cement without pozzolanic cementitious materials. In this type of concrete, carbon dioxide is slowly absorbed to convert the Portlandite into insoluble calcium carbonate (CaCO 3 ), in a process called carbonatation: Ca(OH)2 + CO2 -> CaCO3 + H2O In mineral form, calcium carbonate can exhibit a wide range of hardness depending on how it is formed. At its softest, calcium carbonate can form in concrete as chalk (of hardness 1.0 on Mohs scale).

Like Portlandite, calcium carbonate in mineral form can also be porous, permeable and with a poor resistance to acid attack, which causes it to release carbon dioxide. Pozzolanic concretes, including EMCs, however, continue to consume the soft and porous Portlandite as the hydration process continues, turning it into additional hardened concrete as calcium silicate hydrate (C-S-H) rather than calcium carbonate. This results in a denser, less permeable and more durable concrete.

This reaction is an acid-base reaction between Portlandite and silicic acid (H 4 SiO 4 ) that may be represented as follows: Ca(OH)2 + H4SiO4 -> Ca^2+ + H2SiO4^2- + 2H2O -> CaH2SiO4 * 2H2O   Further, many pozzolans contain aluminate (Al(OH) 4 − ) that will react with Portlandite and water to form: calcium aluminate hydrates, such as calcium aluminium garnet (hydrogrossular: C 4 AH 13 or C 3 AH 6 in cement chemist notation, hardness 7.0 to 7.5 on Mohs scale);   or in combination with silica, to form strätlingite (Ca 2 Al 2 SiO 7 ·8H 2 O or C 2 ASH 8 in cement chemist notation), which geologically can form as xenoliths in basalt as metamorphosed limestone.

Pozzolanic cement chemistry (along with high-aluminate cement chemistry) is complex and per se is not constrained by the foregoing pathways. For example, strätlingite can be formed in a number of ways, including per the following equation which can add to a concrete's strength: C 2 AH 8   +  2CSH  +  AH 3   +  3H    →    C 2 ASH 8     (cement chemist notation) The role of pozzolans in a concrete's chemistry is not fully understood.

For example, strätlingite is metastable, which in a high temperature and water-content environment (that can be generated during the early curing stages of concrete) may of itself yield stable calcium aluminium garnet (see first bullet point above).

This can be represented per the following equation: 3C 2 AH 8     →    2C 3 AH 6   +  AH 3   +  9H    (cement chemist notation) Per the first bullet point, although the inclusion of calcium aluminium garnet per se is not problematic, if it is instead produced by the foregoing pathway, then micro-cracking and strength-loss can occur in the concrete. However, adding high-reactivity pozzolans into the concrete mix prevents such a conversion reaction.

In sum, whereas pozzolans provide a number of chemical pathways to form hardened materials, "high-reactivity" pozzolans such as blast furnace slag (GGBFS) can also stabilise certain pathways. In this context, EMCs made from fly ash have been demonstrated to produce concretes that meet the same characteristics as concretes comprising "120 Slag" (i.e., GGBFS) according to U.S. standard ASTM C989. Portlandite, when exposed to low temperatures, moist conditions and condensation, can react with sulphate ions to cause efflorescence.

In contrast, pozzolanic chemistry reduces the amount of Portlandite available, to reduce the proliferation of efflorescence. \Delta G = G_T^* - G_T   where, for temperature T , the terms G_T^* and G_T are the respective Gibbs values in the processed and unprocessed material. At its simplest, HEBM causes the destruction of crystalline bonds, to increase a material's reactivity.

From the thermodynamic perspective, any subsequent chemical reaction can decrease the excess energy level in the activated-material (i.e. as a reactant) to produce new components comprising both a lower chemical energy and a more stable physical structure. Conversely, to render the pre-processed material into a more reactive physical state, the disordering process during the HEBM process can be justified as being equivalent to a decrystallisation (and hence an entropy increase) that in part yields a volume increase (decrease of bulk density).

A reverse process, sometimes called "relaxation", can be almost immediate (10 −7 to 10 −3 seconds) or take much longer (e.g. 10 6 seconds). Ultimately, any overall retained thermodynamic effect can be justified on the basis that any such reverse process is incapable of reaching an ideal thermodynamic end-state of its own accord. As a result, in the course of the mechanical activation of minerals, reverse "relaxation" processes cannot completely decrease the Gibbs free energy that has been created.

Hence, energy remains in the material, which is stored in the crystal-lattice defects created. \Delta G = \Delta H - T \Delta S    where, \Delta H is the change in enthalpy and \Delta S the change in entropy. \Delta H_T = \Delta H_d + \Delta H_S + \Delta H_A + \Delta H_p   where: \Delta H_d   is a measure of the dislocation density; \Delta H_p   is a measure of new phases (polymorphic transformation); \Delta H_A   is a measure of the formation of amorphous material; \Delta H_S   is a measure of specific surface area.

Because the majority of the work exacted during the EMC Activation process goes to aspect ( \Iota \Iota ) above, \Delta H_S  is trivial. Hence the major functions for the change in enthalpy approximate to: \Delta H _{EMC} \approxeq \Delta H_d + \Delta H_A + \Delta H_p In EMC Activation, the foregoing terms \Delta H_d and \Delta H_A are seen as being particularly prominent because of the nature of the changes in the physical structure observed.

Hence, the change in enthalpy H occasioned during EMC Activation can be approximated to: \Delta H _{EMC} \thickapprox \Delta H_d + \Delta H_A       i.e,    \Delta H_{EMC} \thickapprox (\rho M_V) \frac{b^2\mu_s}{4\pi}\ln \left ( \frac{2(\rho)^{1/2}}{b} \right ) + C_AE_A where: M_V , b , \mu_s and \rho correspond respectively to the molar volume of the material, Burgers vector, shear modulus and dislocation density; C_A and E_A are respectively the concentration of the amorphous phase and molar amorphisation energy.

As a possible explanation of why amorphous silica is more reactive than its crystalline version, thermodynamic treatments may give further insight, even if such approaches cannot fully explain the phenomenon. For example, the so-called "glass transition temperature" increases with an increasing cooling rate q_0 (i.e., dT=\pm q_0dt ) that allows energy to be accumulated as if "frozen in".

Thus, by substantially increasing that cooling rate, "glasses with thermodynamic properties can be obtained, substantially different from those of the initial metastable undercooled liquid". At very high cooling rates, the enthalpy frozen into the resulting vitrified system can be equal to (or exceed) the enthalpy of melting H_m where the cooling rate q_0 is to the order of 10 6 to 10 9 K/s and upwards.

Hence, assuming that the shock-wave dynamics of the EMC Activation process hold true, such that focal nanoscale temperature fluctuations are extremely transient (as described generally per the next section), means that the cooling rates during the HEBM process are to at least similar orders of magnitude, if not more.

Hence: \Delta H _A \geq \Delta H_m (recalling that \Delta H _{EMC} \approxeq \Delta H_d + \Delta H_A + \Delta H_p ) As a result of the rise in H_A , the chemical potential of the system is increased and "frozen in", which gives rise to an increase in any subsequent reactivity. All told, in common with other HEBM processes, EMC Activation causes crystalline destruction because of extremely violent and disruptive factors that are occasioned at the nanoscale of the material being processed.

Although over in short duration and highly focal, the processes are repeated at a high frequency: hence those factors are thought to mimic pressures and temperatures found deep inside the Earth to cause the required phase change.

For example, Peter Thiessen developed the magma-plasma model that assumes localised temperatures—higher than 10 3 kelvins—can be generated at the various impact points to induce a momentary excited plasma state in the material, characterized by the ejection of electrons and photons together with the formation of excited fragments (see diagram above). Experimental data gathered from localised crack-generation, itself an important component of EMC Activation, has confirmed temperatures in this region as long ago as 1975.

F =\left [ \left ( \frac{5m}{8} \right ) ^{3/5} \left ( \frac{2r}{9 \pi^2k^2} \right )^{1/5} \right ]v^{6/5}      where, k = \frac{1 - v^2}{\pi E} where, m is the mass of both balls, r the radius, v the absolute velocity of impact and E the Young's modulus of the balls' material. As can be seen, an increase in velocity of impact increases F . The size and mass of the grinding media also contribute.

F 's denominator term k incorporates E meaning that the nature of the material used for the grinding media is an important factor ( k is ultimately squared in F , so its negative value is of no consequence). More fundamentally, due to the rapid vibration a high acceleration is imparted to the grinding media, whereupon the continuous, short, sharp impacts on the load result in rapid particle-size reduction.

In addition, high pressures and shear stresses facilitate the required phase transition to an amorphous state both at the point of impact and also during the transmission of shock-waves that can yield even greater pressures than the impact itself. For example, the contact time of a two-ball collision can be as short as 20μs, generating a pressure of 3.3 GPa upwards and with an associated ambient temperature increase of 20 kelvins.

Because of the short duration of the impact, the rate of change in momentum is significant—generating a shock wave of duration only 1-100μs but with an associated pressure of 10 GPa upwards and a highly localised and focal temperature (i.e., at the nanoscale) up to several thousands of kelvins. To place this into context, a pressure of 10GPa is equivalent to about 1,000 kilometers of sea water.

As a further example, the impact of two identical steel balls of 2.5 cm diameter of velocity 1 m/s will generate a collision energy density of over 10 9 joules/m 2 , with alumina balls of the same 2.5 cm diameter and velocity of 1 m/s generating an even greater energy density. The collisions occur in a very short timescale and hence the "rate of energy release over the relatively small contact area can be very high".

See also

Background science to EMC Activation: Academic:

Notes

References

External links

, Sweden at lowcarboncement.com Luleå University of Technology, Sweden at LTU.se Future Infrastructure Forum, University of Cambridge, United Kingdom at Fif.construction.cam.ac.uk U.S. Geological Survey (USGS) Cement Statistics and Information at Minerals.usgs.gov U.S. Environmental Protection Agency (EPA), Rule Information for Portland Cement Industry at EPA.gov American Concrete Institute at Concrete.org EDGAR – Emission Database for Global Atmospheric Research at Edgar.jrc.ec.europa.eu Vitruvious: The Ten Books on Architecture online: cross-linked Latin text and English translation at Wbcsdcement.org

Text derived from https://en.wikipedia.org/w/index.php?oldid=1376643046 under CC BY-SA 4.0; modifications have been made.

Sources cited in this revision

36 named source(s) extracted from the cited revision. A source with no author is shown by its publication; nothing is invented.