NASICON

NASICON is an acronym for sodium (Na) super ionic conductor, which usually refers to a family of solids with the chemical formula Na 1+x Zr 2 Si x P 3−x O 12 , 0 −3 S/cm, which rival those of liquid electrolytes.

Uses your system voice; voice and rate in settings.

Snapshot

≈ 4 min read

Names in other languages

No names in other languages are held for this entry yet.

Article bodies are English and are not machine-translated. A name in another language is not a translation of the article.

NASICON is an acronym for sodium (Na) super ionic conductor, which usually refers to a family of solids with the chemical formula Na 1+x Zr 2 Si x P 3−x O 12 , 0 −3 S/cm, which rival those of liquid electrolytes. They are caused by hopping of Na ions among interstitial sites of the NASICON crystal lattice.

Properties

The crystal structure of NASICON compounds was characterized in 1968. It is a covalent network consisting of ZrO 6 octahedra and PO 4 /SiO 4 tetrahedra that share common corners. Sodium ions are located at two types of interstitial positions.

They move among those sites through bottlenecks, whose size, and thus the NASICON electrical conductivity, depends on the NASICON composition, on the site occupancy, and on the oxygen content in the surrounding atmosphere. The conductivity decreases for x 4 Zr 2 Si 3 O 12 , react with molten sodium at 300 °C, and therefore are unsuitable for electric batteries that use sodium as an electrode.

However, a NASICON membrane is being considered for a sodium-sulfur battery where the sodium stays solid. Lithium zirconium phosphate, identified by the formula (LZP), has been extensively studied because of its polymorphism and interesting conduction properties.

At room temperature, LZP has a triclinic crystal structure (C 1 ) and undergoes a phase transition to rhombohedral crystal structure (R 3 c) between 25 and 60 °C. The rhombohedral phase is characterized by higher values of ionic conductivity (8×10 −6 S/cm at 150 °C) compared to the triclinic phase (≈ 8×10 −9 S/cm at room temperature): such difference may be ascribed to the peculiar distorted tetrahedral coordination of lithium ions in the rhombohedral phase, along with the large number of available empty sites. The ionic conductivity of LZP can be enhanced by elemental doping, for example replacing some of the zirconium cations with lanthanum, titanium, or aluminium atoms.

In case of lanthanum doping, the room-temperature ionic conductivity of the material approaches 7.2×10 −5 S/cm. Lithium titanium phosphate, with general formula (LTP or LTPO), is another lithium-containing NASICON material in which TiO 6 octahedra and PO 4 tetrahedra are arranged in a rhombohedral unit cell.

The LTP crystal structure is stable down to 100 K and is characterized by a small coefficient of thermal expansion. LTP shows low ionic conductivity at room temperature, around 10 −6 S/cm; however, it can be effectively increased by elemental substitution with isovalent or aliovalent elements (Al, Cr, Ga, Fe, Sc, In, Lu, Y, La).

The most common derivative of LTP is lithium aluminium titanium phosphate (LATP), whose general formula is . Ionic conductivity values as high as 1.9×10 −3 S/cm can be achieved when the microstructure and the aluminium content (x = 0.3 - 0.5) are optimized.

The increase of conductivity is attributed to the larger number of mobile lithium ions necessary to balance the extra electrical charge after Ti replacement by Al , together with a contraction of the c axis of the LATP unit cell. In spite of attractive conduction properties, LATP is highly unstable in contact with lithium metal, with formation of a lithium-rich phase at the interface and with reduction of Ti to Ti .

Reduction of tetravalent titanium ions proceeds along a single-electron transfer reaction: LiTi2(PO4)3 + Li -> Li2Ti2(PO4)3 Both phenomena are responsible for a significant increase of the electronic conductivity of the LATP material (from 3×10 −9 S/cm to 2.9×10 −6 S/cm), leading to the degradation of the material and to the ultimate cell failure if LATP is used as a solid electrolyte in a lithium-ion battery with metallic lithium as the anode.

Text derived from https://en.wikipedia.org/w/index.php?oldid=1368847044 under CC BY-SA 4.0; modifications have been made.

Sources cited in this revision

15 named source(s) extracted from the cited revision. A source with no author is shown by its publication; nothing is invented.