Palmqvist method

The Palmqvist method, or the Palmqvist toughness test, (after Sven Robert Palmqvist) is a common method to determine the fracture toughness for cemented carbides.

Uses your system voice; voice and rate in settings.

Snapshot

≈ 1 min read

Names in other languages

No names in other languages are held for this entry yet.

Article bodies are English and are not machine-translated. A name in another language is not a translation of the article.

The Palmqvist method, or the Palmqvist toughness test, (after Sven Robert Palmqvist) is a common method to determine the fracture toughness for cemented carbides. In this case, the material's fracture toughness is given by the critical stress intensity factor K Ic . It was developed c. 1962.

Approach

The Palmqvist-method uses the lengths of the cracks from a number of Vickers indentions to determine the fracture toughness. The Palmqvist fracture toughness is given by K_{\text{Ic}} = 0.0028\sqrt{\text{HV}}\sqrt{\frac{P}{T}} in units of MPa \sqrt{\text{m}} , where HV is the Vickers hardness in N/mm 2 (or MPa) (i.e., 9.81 x numerical HV), P is the indentation load in N (typically 30 kgf is used) and T is the total crack length (mm) after application of the indenter.

Notes

ISO 28079:2009, Palmqvist toughness test

Text derived from https://en.wikipedia.org/w/index.php?oldid=1329411061 under CC BY-SA 4.0; modifications have been made.

Provenance

snapshot enwiki-001329411061 · captured 1766704328.0 · version history

Cite this page as: encyclopegia.org, “Palmqvist method”, snapshot enwiki-001329411061. https://encyclopegia.org/a/palmqvist-method

Sources cited in this revision

1 named source(s) extracted from the cited revision. A source with no author is shown by its publication; nothing is invented.