Stöber process
≈ 7 min read
Names in other languages
- DeutschStöber-Synthese
- EnglishStöber process
- Polskiproces Stöbera
- 日本語ストーバー法
- 中文史托伯法
Article bodies are English and are not machine-translated. A name in another language is not a translation of the article.
The Stöber process is a chemical process used to prepare silica ( ) particles of controllable and uniform size for applications in materials science. It was pioneering when it was reported by Werner Stöber and his team in 1968, and remains today the most widely used wet chemistry synthetic approach to silica nanoparticles. It is an example of a sol-gel process wherein a molecular precursor (typically tetraethylorthosilicate) is first reacted with water in an alcoholic solution, the resulting molecules then joining to build larger structures.
How it works
The reaction produces silica particles with diameters ranging from 50 to 2000 nm, depending on conditions. The process has been actively researched since its discovery, including efforts to understand its kinetics and mechanism a particle aggregation model was found to be a better fit for the experimental data than the initially hypothesized LaMer model.
The newly acquired understanding has enabled researchers to exert a high degree of control over particle size and distribution and to fine-tune the physical properties of the resulting material in order to suit intended applications. In 1999 a two-stage modification was reported that allowed the controlled formation of silica particles with small holes. The process is undertaken at low pH in the presence of a surface-active molecule.…
The Stöber process is a chemical process used to prepare silica ( ) particles of controllable and uniform size for applications in materials science. It was pioneering when it was reported by Werner Stöber and his team in 1968, and remains today the most widely used wet chemistry synthetic approach to silica nanoparticles. It is an example of a sol-gel process wherein a molecular precursor (typically tetraethylorthosilicate) is first reacted with water in an alcoholic solution, the resulting molecules then joining to build larger structures.
The reaction produces silica particles with diameters ranging from 50 to 2000 nm, depending on conditions. The process has been actively researched since its discovery, including efforts to understand its kinetics and mechanism a particle aggregation model was found to be a better fit for the experimental data than the initially hypothesized LaMer model.
The newly acquired understanding has enabled researchers to exert a high degree of control over particle size and distribution and to fine-tune the physical properties of the resulting material in order to suit intended applications. In 1999 a two-stage modification was reported that allowed the controlled formation of silica particles with small holes. The process is undertaken at low pH in the presence of a surface-active molecule.
The hydrolysis step is completed with the formation of a microemulsion before adding sodium fluoride to nucleate the condensation process. The non-ionic surfactant is burned away to produce empty pores, increasing the surface area and altering the surface characteristics of the resulting particles, allowing for much greater control over the physical properties of the material.
Development work has also been undertaken for larger pore structures such as macroporous monoliths, shell-core particles based on polystyrene, cyclen, or polyamines, and carbon spheres. Silica produced using the Stöber process is an ideal material to serve as a model for studying colloid phenomena because of the monodispersity (uniformity) of its particle sizes. Nanoparticles prepared using the Stöber process have found applications including in the delivery of medications to within cellular structures and in the preparation of biosensors.
Porous silica Stöber materials have applications in catalysis and liquid chromatography due to their high surface area and their uniform, tunable, and highly ordered pore structures. Highly effective thermal insulators known as aerogels can also be prepared using Stöber methods, and Stöber techniques have been applied to prepare non-silica aerogel systems. Applying supercritical drying techniques, a Stöber silica aerogel with a specific surface area of 700 m 2 ⋅g −1 and a density of 0.040 g⋅cm −3 can be prepared.
NASA has prepared silica aerogels with a Stöber-process approach for both the Mars Pathfinder and Stardust missions. J = g_s(e^{-k_1t}-e^{-k_2t}) where J is the nucleation rate, k 1 and k 2 are rate constants based on the concentrations of H 2 O and NH 3 and g s is the normalization factor based on the amount of silica precursor. Adjusting the concentration ratios of these compounds directly influences the rate at which nucleation sites are produced. Merging of nucleation sites between particles is influenced by their interaction energies.
The total interaction energy is dependent on three forces: electrostatic repulsion of like charges, van der Waals attraction between particles, and the effects of solvation. These interaction energies (equations below) describe the particle aggregation process and demonstrate why the Stöber process produces particles that are uniform in size.
V_T = V_{\text{vdw}} + V_{\text{elec}} + V_{\text{solv}} The van der Waals attraction forces are governed by the following equation: V_{\text{vdw}}=-\frac{A_\text{H}}{6}\left[\frac{2a_1a_2}{R^2-(a_1+a_2)^2}+\frac{2a_1a_2}{R^2-(a_1-a_2)^2}+\ln\frac{R^2-(a_1+a_2)^2}{R^2-(a_1-a_2)^2}\right] where A H is the Hamaker constant, R is the distance between the centers of the two particles and a 1 , a 2 are the radii of the two particles.
For electrostatic repulsion force the equation is as follows: V_{\text{elec}} = 4\pi\varepsilon a_1a_2Y_1Y_2\left(\frac{k_\text{B}T}{e}\right)^2 \frac{e^{-\kappa x}}{x+a_1+a_2} where Y_i = \frac{8\tanh\frac{e\varphi_0}{4k_\text{B}T}}{1+\sqrt{1-\frac{2\kappa a_i+1}{(\kappa a_i+1)^2}\tanh^2\frac{e\varphi_0}{4k_\text{B}T}}} Where ε is the dielectric constant of the medium, k B is the Boltzmann constant, e is the elementary charge, T is the absolute temperature, κ is the inverse Debye length for a 1:1 electrolyte, x is the (variable) distance between the particles, and φ 0 is the surface potential.
The final component of the total interaction energy is the solvation repulsion which is as follows: V_{\text{solv}}=\pi A_\text{s}L\left[\frac{2a_1a_2}{a_1+a_2}\right]e^\frac{-(R-a_1-a_2)}{L} where A s is the pre-exponential factor (1.5 × 10 −3 J⋅m −2 ) and L is the decay length (1 × 10 −9 m). This model for controlled growth aggregation fits with experimental observations from small-angle X-ray scattering techniques and accurately predicts particle sizing based on initial conditions.
Evidence and sources
In addition, experimental data from techniques including microgravity analysis and variable pH analysis agree with predictions from the aggregate growth model.
Text derived from https://en.wikipedia.org/w/index.php?oldid=1372676356 under CC BY-SA 4.0; modifications have been made.