Delamination
under compression load Delamination is a mode of failure where a material fractures into layers.[src] A variety of materials, including laminate composites and concrete, can fail by delamination.[src] Processing can create layers in materials, such as steel formed by rolling and plastics and metals from 3D printing which can fail from layer separation.[src] Also, surface coatings, such as paints and films, can delaminate from the coated substrate.[src] In laminated composites, the adhesion between layers often fails first, causing the layers to separate.[src] For example, in fiber-reinforced plastics, sheets of high strength reinforcement (e.g., carbon fiber, fiberglass) are bound together by a much weaker polymer matrix (e.g., epoxy).[src] In particular, loads applied perpendicular to the high strength layers, and shear loads can cause the polymer matrix to fracture or the fiber reinforcement to debond from the polymer.[src] Delamination also occurs in reinforced concrete when metal reinforcements near the surface corrode.[src] The oxidized metal has a larger volume causing stresses when confined by the concrete.[src] When the stresses exceed the strength of the concrete, cracks can form and spread to join with neighboring cracks caused by corroded rebar creating a fracture plane that runs parallel to the surface.[src] Once the fracture plane has developed, the concrete at the surface can separate from the substrate.…[src]
under compression load]] Delamination is a mode of failure where a material fractures into layers.[src] A variety of materials, including laminate composites and concrete, can fail by delamination.[src] Processing can create layers in materials, such as steel formed by rolling and plastics and metals from 3D printing which can fail from layer separation.[src] Also, surface coatings, such as paints and films, can delaminate from the coated substrate.[src] In laminated composites, the adhesion between layers often fails first, causing the layers to separate.[src] For example, in fiber-reinforced plastics, sheets of high strength reinforcement (e.g., carbon fiber, fiberglass) are bound together by a much weaker polymer matrix (e.g., epoxy).[src] In particular, loads applied perpendicular to the high strength layers, and shear loads can cause the polymer matrix to fracture or the fiber reinforcement to debond from the polymer.[src] Delamination also occurs in reinforced concrete when metal reinforcements near the surface corrode.[src] The oxidized metal has a larger volume causing stresses when confined by the concrete.[src] When the stresses exceed the strength of the concrete, cracks can form and spread to join with neighboring cracks caused by corroded rebar creating a fracture plane that runs parallel to the surface.[src] Once the fracture plane has developed, the concrete at the surface can separate from the substrate.[src] Processing can create layers in materials which can fail by delamination.[src] In concrete, surfaces can flake off from improper finishing.[src] If the surface is finished and densified by troweling while the underlying concrete is bleeding water and air, the dense top layer may separate from the water and air pushing upwards.[src] In steels, rolling can create a microstructure when the microscopic grains are oriented in flat sheets which can fracture into layers.[src] Also, certain 3D printing methods (e.g., fused deposition) builds parts in layers that can delaminate during printing or use.[src] When printing thermoplastics with fused deposition, cooling a hot layer of plastic applied to a cold substrate layer can cause bending due to differential thermal contraction and layer separation.[src] G_Q = \frac{3mP^{2}_{\max}a^{2}_{0}}{2B} where B is the thickness of the specimen and P_{\max} is the max load and m is a fitting parameter.[src] m is determined by experimental results with a least squares fit of compliance C vs.[src] the crack length cubed a^3 with the form of C = A + ma^3 .[src] The candidate fracture toughness G_Q equals the mode II fracture toughness G_{IIc} if strain energy release rate falls within certain percentage of G_Q at different crack lengths specified by ASTM.[src] \frac{P}{Q} = \frac{S_2}{S_1} = \lambda , where S_1 and S_2 are the lengths from the inner pin to the applied point load and from the outer pin to the applied point load, respectively.[src] The normal stress in the sample \sigma_{xx} is maximized at the locations of the inner pins, and is equivalent to \sigma_{xx} = \frac{6(\lambda-1)FL}{(1+\lambda^2)bt} , where F is the total applied load on the sample, L is the sample length, b is the sample width (into the page as seen in a 2D free-body diagram), and t is the sample thickness.[src] The shear stress \sigma_{xz} in the sample is maximized in between the inner span of the pins and is given by \sigma_{xz} = \frac{3(1- \lambda)F}{2(1+ \lambda)bt} .[src] The ratio of normal to shear stress in the sample C is given by C = \frac{\sigma_{xx}}{\sigma_{xz}} = \frac{4L}{(1+\lambda)t} .[src] This ratio is dependent both on the loading factor of the sample and its length-thickness ratio; both of these quantities are important in determining the mode of failure of the sample in testing.[src]
37 sentences · 37 cited inline · 0 references stored
References
No reference rows published for this article.
Cite this article
MLA
"Delamination." encyclopegia.org, 2025, https://encyclopegia.org/wiki/delamination. Accessed 26 November 2026.
Chicago
"Delamination." encyclopegia.org. Accessed November 26, 2026. https://encyclopegia.org/wiki/delamination.
APA
encyclopegia.org. (2025). Delamination. Retrieved November 26, 2026, from https://encyclopegia.org/wiki/delamination
Accessed November 26, 2026 · CC BY-SA 4.0 · citation page · JSON