Semi-solid metal casting
Semi-solid metal casting (SSM) is a near net shape variant of die casting.[src] The process is used today with non-ferrous metals, such as aluminium, copper, and magnesium.[src] It can work with higher temperature alloys that lack suitable die materials.[src] The process combines the advantages of casting and forging.[src] The process is named after the fluid property thixotropy, which is the phenomenon that allows this process to work.[src] Thixotropic fluids flow when sheared, but thicken when standing.[src] The potential for this type of process was first recognized in the early 1970s.[src] Its three variants are thixocasting, rheocasting, and thixomolding.[src] SIMA refers to a specialized process to prepare aluminum alloys for thixocasting using hot and cold working.[src] SSM is done at a temperature that puts the metal between its liquidus and solidus temperature, ideally 30 to 65% solid.[src] The mixture must have low viscosity to be usable, and to reach this low viscosity the material needs a globular primary surrounded by the liquid phase.[src] The temperature range depends on the material and for aluminum alloys can be as much as 50 °C, but for narrow melting range copper alloys can be only several tenths of a degree.[src] SSM is typically used for high-end applications.…[src]
Semi-solid metal casting (SSM) is a near net shape variant of die casting.[src] The process is used today with non-ferrous metals, such as aluminium, copper, and magnesium.[src] It can work with higher temperature alloys that lack suitable die materials.[src] The process combines the advantages of casting and forging.[src] The process is named after the fluid property thixotropy, which is the phenomenon that allows this process to work.[src] Thixotropic fluids flow when sheared, but thicken when standing.[src] The potential for this type of process was first recognized in the early 1970s.[src] Its three variants are thixocasting, rheocasting, and thixomolding.[src] SIMA refers to a specialized process to prepare aluminum alloys for thixocasting using hot and cold working.[src] SSM is done at a temperature that puts the metal between its liquidus and solidus temperature, ideally 30 to 65% solid.[src] The mixture must have low viscosity to be usable, and to reach this low viscosity the material needs a globular primary surrounded by the liquid phase.[src] The temperature range depends on the material and for aluminum alloys can be as much as 50 °C, but for narrow melting range copper alloys can be only several tenths of a degree.[src] SSM is typically used for high-end applications.[src] For aluminum alloys, typical parts include structural medical and aerospace parts, pressure containing parts, defense parts, engine mounts, air manifold sensor harnesses, engine blocks, and oil pump filter housings.[src] ==Processes== Four techniques involve semi-solid castings.[src] For aluminum alloys the more common processes are thixocasting, rheocasting, and SIMA.[src] With magnesium alloys, the most common process is thixomolding.[src] ===Thixocasting=== Thixocasting utilizes a pre-cast billet with a non-dendritic microstructure that is normally produced by vigorously stirring the melt as the bar is being cast.[src] Induction heating is normally used to re-heat the billets to the semi-solid temperature range, and die casting machines are used to inject the semi-solid material into hardened steel dies.[src] Thixocasting is employed commercially.[src] Thixocasting can produce high quality components due to the product consistency that results from using pre-cast billets manufactured under the same ideal continuous processing conditions that are employed to make forging or rolling stock.[src] The main disadvantage is that it is expensive due to the specialized billets, although facilities with in house magnetohydrodynamic continuous casting capabilities can recycle 100% of in-house returns.[src] Other disadvantages include support for a limited number of alloys, and in-house magnetohydrodynamic casting capability to directly reuse scrap.[src] ===Rheocasting=== Rheocasting develops the semi-solid slurry from the molten metal produced in a typical die casting furnace.[src] This allows less expensive feedstock, in the form of typical die casting alloys, and allows for direct recycling.[src] However, rheocasting also poses process control issues such that after an initial surge of activity, very little material is processed via rheocasting.[src] ===Thixomolding=== For magnesium alloys, thixomolding uses a machine similar to injection molding.[src] In a single step process, room temperature magnesium alloy chips are fed into the back end of a heated barrel through a volumetric feeder.[src] The barrel maintains an argon atmosphere to prevent oxidation.[src] A screw conveyor located inside the barrel feeds the magnesium chips forward as they are heated into the semi-solid temperature range.[src] The screw rotation provides the necessary shearing force to generate the globular structure needed for semi-solid casting.[src] Once enough slurry has accumulated, the screw moves forward to inject the slurry into a steel die.[src] The flow of the material is less turbulent, creating near-zero porosity.[src] The slower velocity of the material into the die extends die life by more than 2x.[src] ===Strain-induced melt-activated (SIMA)=== In the SIMA method the material is first heated to the SMM temperature.[src] As it nears the solidus temperature the grains recrystallize to form a fine grain structure.[src] After the solidus temperature is passed the grain boundaries melt to form the SSM microstructure.[src] For this method to work the material should be extruded or cold rolled in the half-hard tempered state.[src] This method supports bar diameters only smaller than .[src] ==Advantages== High consolidation pressures are used to produce high integrity parts.[src] The advantages of semi-solid casting are: Complex parts produced net shape Pore free Reduced shrinkage Mechanical performance Pressure tightness Tight tolerances Thin walls Heat treatable (T4/T5/T6) Good surface finish Lower casting temperature Uses conventional tool steel materials Ease of automation Production rates equal to or better than die casting rates Uniform microstructure.[src] Relatively insensitive to ambient temperature since small heat losses cause only minor changes in fraction solid.[src] ==Disadvantages== Production facilities require a higher degree of control over process conditions, Requires higher final injection pressures Requires lower injection velocities.[src] Requires on-site magneto-hydrodynamic continuous casting capabilities in order to completely recycle in-house material returns.[src] Lack of suitable high temperature die materials limits the casting of high melting point metals, such as tool steel and stellite, to experimental applications.[src] ==See also== Metal injection molding Spray forming ==References== ===Notes=== ===Bibliography=== .[src] ==External links== Video of an automatic forging cell for SSM pt:Fundição injetada[src]
60 sentences · 60 cited inline · 0 references stored
References
No reference rows published for this article.
Cite this article
MLA
"Semi-solid metal casting." encyclopegia.org, 2026, https://encyclopegia.org/wiki/semi-solid-metal-casting. Accessed 29 November 2026.
Chicago
"Semi-solid metal casting." encyclopegia.org. Accessed November 29, 2026. https://encyclopegia.org/wiki/semi-solid-metal-casting.
APA
encyclopegia.org. (2026). Semi-solid metal casting. Retrieved November 29, 2026, from https://encyclopegia.org/wiki/semi-solid-metal-casting
Accessed November 29, 2026 · CC BY-SA 4.0 · citation page · JSON