An AFm phase is an "alumina, ferric oxide, monosubstituted" phase, or aluminate ferrite monosubstituted, or , mono, in cement chemist notation (CCN). AFm phases are important hydration products in the hydration of Portland cements and hydraulic cements.

They are crystalline hydrates with generic, simplified, formula , where: * CaO, , represent calcium oxide, aluminium oxide, and ferric oxide, respectively; * CaX represents a calcium salt, where X replaces an oxide ion; * X is the substituted anion in CaX: – divalent ( , ...) with y = 1, or; – monovalent ( , ...) with y = 2. * n represents the number of water molecules in the hydrate and may be comprised between 13 and 19. AFm form inter alia when tricalcium aluminate in CCN, reacts with dissolved calcium sulfate ( ), or calcium carbonate ( ).

As the sulfate form is the dominant one in AFm phases in the hardened cement paste (HCP) in concrete, AFm is often simply referred to as Aluminate Ferrite monosulfate or calcium aluminate monosulfate. However, carbonate-AFm phases also exist (monocarbonate and hemicarbonate) and are thermodynamically more stable than the sulfate-AFm phase. During concrete carbonation by the atmospheric , sulfate-AFm phase is also slowly transformed into carbonate-AFm phases.

An AFm phase is an "alumina, ferric oxide, monosubstituted" phase, or aluminate ferrite monosubstituted, or , mono, in cement chemist notation (CCN). AFm phases are important hydration products in the hydration of Portland cements and hydraulic cements.

They are crystalline hydrates with generic, simplified, formula , where: CaO, , represent calcium oxide, aluminium oxide, and ferric oxide, respectively; CaX represents a calcium salt, where X replaces an oxide ion; X is the substituted anion in CaX: – divalent ( , ...) with y = 1, or; – monovalent ( , ...) with y = 2. n represents the number of water molecules in the hydrate and may be comprised between 13 and 19. AFm form inter alia when tricalcium aluminate in CCN, reacts with dissolved calcium sulfate ( ), or calcium carbonate ( ).

As the sulfate form is the dominant one in AFm phases in the hardened cement paste (HCP) in concrete, AFm is often simply referred to as Aluminate Ferrite monosulfate or calcium aluminate monosulfate. However, carbonate-AFm phases also exist (monocarbonate and hemicarbonate) and are thermodynamically more stable than the sulfate-AFm phase. During concrete carbonation by the atmospheric , sulfate-AFm phase is also slowly transformed into carbonate-AFm phases.

See also

AFt phases Concrete degradation#Chloride attack Layered double hydroxides (LDH) Friedel's salt Ettringite (AFt) Pitting corrosion of rebar induced by chloride attack

References

Further reading

Text derived from https://en.wikipedia.org/w/index.php?oldid=1368620792 under CC BY-SA 4.0; modifications have been made.

Sources cited in this revision

7 named source(s) extracted from the cited revision. A source with no author is shown by its publication; nothing is invented.